K-Resin KR05

K-Resin® KR05 is easily processed on injection molding, blow molding or extrusion and thermoforming equipment, and it gives excellent part detail on fast production cycles. K-Resin® KR05 has outstanding retention and excellent color consistaency after gamma, E-beam, EtO sterilization. K-Resin® KR05 is a part of the Essential HD Package that can be provided with EU and US food contact statements, USP Class VI, ISO 10993 compliance.

Key Features

  • Excellent Clarity
  • Good Stiffness & Toughness
  • Good Formability
  • High Surface Gloss
  • Excellent Bonding Performance
  • Gamma, E-beam, EtO Sterilization

Applications

  • Medical Devices
  • Molded Box and Containers
  • Blow Moldings
  • Portion Packages
  • Blister Packaging
  • Grade Version
  • Properties

    คุณสมบัติของ

    ค่าทั่วไปสำหรับผลิตภัณฑ์ที่ไม่ทำสีที่ 23 องศาเซลเซียส วิธีการทดสอบ หน่วย ค่า
    คุณสมบัติการเปลี่ยนรูปและการไหล
    Melt Flow Rate, 200 °C/5 kg ASTM D 1238 g/10 min 7.5
    คุณสมบัติทางกล
    Instrumented Dart Impact (total energy) ASTM D 3763 in-lbs 354
    Tensile Modulus ASTM D 638 psi x 10³ 220
    Tensile Stress at Yield, 23 °C ASTM D 638 psi 3800
    Tensile Strain at Break, 23 °C ASTM D 638 % 230
    Flexural Strength, 23 °C ASTM D 790 psi 5400
    Flexural Modulus, 23 °C ASTM D 790 psi x 10³ 260
    Hardness, Shore D ASTM D 2240 - 63
    คุณสมบัติทางความร้อน
    Vicat Softening Temperature, B/1 ( 120 °C/h, 10N) ASTM D 1525 °F 185
    DTUL @ 264 psi - Annealed ASTM D 648 °F 144
    คุณสมบัติอื่น ๆ
    Light Transmission at 550 nm ASTM D 1003 % 92
    Gardner Gloss (mold temperature 100°F) ASTM D2457 % 162
    Haze ASTM D 1003 % 1
    Other Properties
    Density (ASTM ) ASTM D 792 g/cm³ 1.01
    Moisture Absorption ASTM D570 % 0.09

    The nominal properties herein are typical of the product but do not reflect normal testing variance and therefore should not be used for specification purposes. Values are rounded.
    The nominal properties herein are typical of the product but do not reflect normal testing variance and therefore should not be used for specification purposes. Values are rounded.\n(Tensile Yield Strength/Tensile Elongation @ Break) = Type 1 @ 2 in/min (

  • Processing

    กำลังประมวลผล

  • Safety Data Sheet