Products

TERLURAN GP-22

Terluran® GP-22 is an easy-flow, general purpose injection molding grade with high resistance to impact and heat distortion; intended for a wide range of applications, particularly in the housings sector.

Key Features

  • Excellent colorability
  • Medium flow
  • Good impact resistance
  • Good heat distortion resistance
  • High quality surface finish and gloss
  • Great mechanical strength and rigidity

Applications

  • Injection molding
  • Appliance housings
  • Household and sanitary appliances
  • Toys
  • Automotive components
  • Consumer products
  • Grade Version
  • Properties

    Properties of TERLURAN GP-22

    Property, Test Condition Standard Unit Values
    Rheological Properties
    Melt Volume Rate 220 °C/10 kg ISO 1133 cm³/10 min 19
    Mechanical Properties
    Izod Notched Impact Strength, 23 °C ISO 180/A kJ/m² 26
    Izod Notched Impact Strength, -30 °C ISO 180/A kJ/m² 8
    Charpy Notched Impact Strength, 23° C ISO 179/1eA kJ/m² 22
    Charpy Notched Impact Strength, -30 °C ISO 179/1eA kJ/m² 8
    Charpy Unnotched, 23 °C ISO 179/1eU kJ/m² 180
    Charpy Unnotched, -30 °C ISO 179/1eU kJ/m² 100
    Tensile Stress at Yield, 23 °C ISO 527 MPa 45
    Tensile Strain at Yield, 23 °C ISO 527 % 2.6
    Tensile Modulus ISO 527 MPa 2300
    Nominal Strain at Break, 23 °C ISO 527 % 10
    Flexural Strength, 23 °C ISO 178 MPa 65
    Hardness, Ball Indentation ISO 2039-1 MPa 97
    Thermal Properties
    Vicat Softening Temperature VST/B/50 (50N, 50 °C/h) ISO 306 °C 96
    Vicat Softening Temperature, VST/A/50 (10N, 50 °C/h) ISO 306 °C 105
    Heat Deflection Temperature A; (annealed 4 h/80 °C; 1.8 MPa) ISO 75 °C 94
    Heat Deflection Temperature B; (annealed 4 h/80 °C; 0.45 MPa) ISO 75 °C 99
    Coefficient of Linear Thermal Expansion ISO 11359 10-6/°C 80 - 110
    Thermal Conductivity ISO 22007-4 W/(m K) 0.17
    Electrical Properties
    Dissipation Factor (100 Hz) IEC 62631-2-1 10-4 48
    Dissipation Factor (1 MHz) IEC 62631-2-1 10-4 79
    Relative Permittivity (100 Hz) IEC 62631-2-1 - 2.9
    Relative Permittivity (1 MHz) IEC 62631-2-1 - 2.8
    Volume Resistivity IEC 62631-3-1 Ω*m >1013
    Surface Resistivity IEC 62631-3-1 Ω >1013
    Other Properties
    Density ISO 1183 kg/m³ 1040
    Water Absorption, Saturated at 23 °C ISO 62 % 1
    Moisture Absorption, Equilibrium 23 °C/50% RH ISO 62 % 0.22
    Yellowness Index DIN 6167 - 13
    Processing
    Linear Mold Shrinkage ISO 294-4 % 0.4 - 0.7
    Melt Temperature Range ISO 294 °C 220 - 260
    Mold Temperature Range ISO 294 °C 30 - 80
    Injection Velocity ISO 294 mm/s 200
    Drying Temperature - °C 80
    Drying Time - h 2 - 4

    Typical values for uncolored products
    Please note that all processing data stated are only indicative and may vary depending on the individual processing complexities.
    Please consult our local sales or technical representatives for details.

  • Processing

    Processing of TERLURAN GP-22

  • Safety Data Sheet