K-Resin KR52
K-Resin® KR52 is designed for a shrink sleeve film application. K-Resin® KR52 offers high clarity, stiffness, gloss and excellent printability.
Key Features
- High Clarity and Gloss
- Good Stiffness
- Excellent Printability
- Up to 80% Shrinkage at 100°C
Applications
- Shrink Sleeve Labels
- Multi-layer Films
- Tamper Evident Bands
- Roll-Fed Labels
Industries
-
Grade Version
Please Sign in or Register with INEOS Styrolution to download REACH and other Regulatory Documents
New to INEOS Styrolution? Registration
-
Properties
Properties of K-Resin KR52
Property, Test Condition Standard Unit Values Rheological Properties Melt Volume Rate, 200 °C/5 kg ISO 1133 cm³/10 min 8 Mechanical Properties Izod Notched Impact Strength, 23 °C ISO 180/A kJ/m² 3 Charpy Notched Impact Strength, 23° C ISO 179/1eA kJ/m² 2 Charpy Unnotched, 23 °C ISO 179/1eU kJ/m² 20 Tensile Stress at Yield, 23 °C ISO 527 MPa 35 Tensile Stress at Break, 23 °C ISO 527 MPa 15 Tensile Strain at Break, 23 °C ISO 527 % 20 Tensile Modulus ISO 527 MPa 1500 Flexural Strength, 23 °C ISO 178 MPa 45 Flexural Modulus, 23 °C ISO 178 MPa 1400 Hardness, Shore D ISO 868 - 70 Thermal Properties Vicat Softening Temperature VST/B/50 (50N, 50 °C/h) ISO 306 °C 60 Vicat Softening Temperature, VST/A/120 (10N, 120 °C/h) ISO 306 °C 65 Heat Deflection Temperature A; (annealed 4 h/80 °C; 1.8 MPa) ISO 75 °C 50 Heat Deflection Temperature B; (annealed 4 h/80 °C; 0.45 MPa) ISO 75 °C 55 Optical Properties Refractive Index, Sodium D Line ISO 489 - 1.57 Light Transmission at 550 nm ASTM D 1003 % 91 Haze ASTM D 1003 % < 1.5 Other Properties Density ISO 1183 kg/m³ 1010 Moisture Absorption, Equilibrium 23 °C/50% RH ISO 62 % 0.07 Processing Linear Mold Shrinkage ISO 294-4 % 0.3 - 1 Melt Temperature Range ISO 294 °C 180 - 220 Mold Temperature Range ISO 294 °C 30 - 50 The nominal properties herein are typical of the product but do not reflect normal testing variance and therefore should not be used for specification purposes. Values are rounded.
Typical cast film properties with 2% impact polystyrene, 2 mil (0.05 mm) (10 mil cast film oriented/tentered 5:1 in the Transverse Direction).
[Vicat Softening Point] = Injection Molded Specimen. -
Processing
Processing of K-Resin KR52
-
Safety Data Sheet