TERBLEND N NM-11
The product line Terblend® N, comprising blends of ABS with PA 6, provides very good mechanical properties, a high melt flow, and very good chemical resistance provided by the polyamide component. Parts from Terblend® have acoustic dampening properties and show in unpainted, textured surfaces a nice matt appearance. Terblend® N NM-11 provides balanced properties and keeps its high impact properties also in combination with a very high concentration of colorants. Its rather low melt flow makes it also well suitable for extrusion applications.
Key Features
- Balanced properties
- Chemical resistance
- Well extrudable
- High surface quality
- Impact strength
Applications
- Shaving systems
- Bicycle/ E-bicycle parts
- Helmets
- Extruded sheets & profiles
Industries
-
Grade Version
Please Sign in or Register with INEOS Styrolution to download REACH and other Regulatory Documents
เพิ่งเข้ามาใหม่ ที่สไตโรลูชั่น ใช่ไหม? ลงทะเบียน ทะเบียน
-
Properties
คุณสมบัติของ
ค่าทั่วไปสำหรับผลิตภัณฑ์ที่ไม่ทำสีที่ 23 องศาเซลเซียส วิธีการทดสอบ หน่วย ค่า คุณสมบัติการเปลี่ยนรูปและการไหล Melt Volume Rate, 240 °C/10 kg ISO 1133 cm³/10 min 30 คุณสมบัติทางกล Charpy Notched Impact Strength, 23° C ISO 179/1eA kJ/m² 65 Charpy Notched Impact Strength, -30 °C ISO 179/1eA kJ/m² 15 Izod Notched Impact Strength, 23 °C ISO 180/A kJ/m² 65 Izod Notched Impact Strength, -30 °C ISO 180/A kJ/m² 15 Tensile Modulus ISO 527 MPa 2000 Tensile Stress at Yield, 23 °C ISO 527 MPa 43 Tensile Strain at Yield, 23 °C ISO 527 % 3.5 Tensile Stress at Break, 23 °C ISO 527 MPa 31.00 Tensile Strain at Break, 23 °C ISO 527 % > 50 Nominal Strain at Break, 23 °C ISO 527 % > 50 Tensile Modulus after Moisture Absorption, Equilibrium 23 °C/50% RH ISO 527 MPa 1400 Tensile Stress at Yield after Moisture Absorption, Equilibrium 23 °C/50% RH ISO 527 MPa 34 Tensile Strain at Yield after Moisture Absorption, Equilibrium 23 °C/50% RH ISO 527 % 5.5 Nominal Strain at Break after Moisture Absorption, Equilibrium 23 °C/50% RH ISO 527 % > 50 Flexural Modulus, 23 °C ISO 178 MPa 1800 Flexural Strength, 23 °C ISO 178 MPa 62 Hardness, Ball Indentation ISO 2039-1 MPa 86 คุณสมบัติทางความร้อน Vicat Softening Temperature VST/B/50 (50N, 50 °C/h) ISO 306 °C 102 Heat Deflection Temperature A; (annealed 4 h/80 °C; 1.8 MPa) ISO 75 °C 85 Heat Deflection Temperature B; (annealed 4 h/80 °C; 0.45 MPa) ISO 75 °C 97 Coefficient of Linear Thermal Expansion ISO 11359 10-6/°C 100 Other Properties Density ISO 1183 kg/m³ 1070 UL94 rating at 1.5 mm thickness IEC 60695-11-10 - HB Glow wire test (GWFI), 2.0 mm IEC 60695-2-12 °C 650 Moisture Absorption, Equilibrium 23 °C/50% RH ISO 62 % 1.2 Processing Linear Mold Shrinkage ISO 294-4 % 0.7 - 0.9 Melt Temperature Range ISO 294 °C 240 - 270 Mold Temperature Range ISO 294 °C 60 - 80 Drying Temperature - °C 80 - 90 Drying Time - h 4 - 8 Typical values for uncolored products
Please note that all processing data stated are only indicative and may vary depending on the individual processing complexities.